I experienced that electroless copper will plate more on teflon or fibre

glass than the copper surface on a panel. That is the PTH wall thickness

of electroless copper plated is more than that is plated on the surface

of the panel which is copper. PTH may have 65 u in. but the surface with

the final thickness of copper minus the original copper thickness is not

65 u in. Can any one help me with that?

Thanks!

my e-mail : [log in to unmask]

Francis

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2