Raul,
Not a practise I would recommend. We have done it once on request from
a customer. If you decide to do it beware of the following:
Different sockets will transfer heat differently. If heat transfer is too
efficient , and the part you are plugging has solder finished leads then
you may reflow the solder. Also some sockets may allow solder wicking up
the socket pins to the leads of the part (seems to be less of a problem on
machined pins).
If you really want to do this then I would suggest a trial run to see if
problems arise before proceeding full steam.
Regards Evan
Evan Jones
Manufacturing/Test Engineer
Bluegum Technology Pty Ltd
PO Box 609, Wangaratta, Australia, 3676
Ph: 61 3 5720 2539 Fax: 61 3 5720 2412
Internet: [log in to unmask]
Raul Cantero <[log in to unmask]> on 08/01/99 08:46:27
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Raul Cantero <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Evan Jones/BGT)
Subject: [TN] Programmed parts in sockets
Does anyone have any experience inserting programmed parts in sockets PRIOR
to wave soldering the socket into the PWA????
Ra
úl Cantero
Business e-mail: [log in to unmask]
Personal e-mail: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
|
|
|