Hi technetters ,
What are the existing and working technologies for electrolytic copper and
tin lead plating of blind vias , laser drilled ?
We are testing now making tests with 0.2 mm diameter , 0.3 mm deep laser
drilled vias . The stage of permanganate desmear and electroless copper
plating was performed in vertical line without special efforts . We tried
different current densities in vertical electrolylic stage , but we got very
poor copper distribution along the wall : 20 microns in the upper part , 5
microns on the bottom and on the lower part of the wall . We just presume ,
tha the same problem will be for tin-lead stage of pattern plating .
Best regards and Happy New Year 1999 !
Edward Szpruch
Eltek Ltd - Israel
e-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|