Hi Technetters,
For the Electroless Ni-Immersion Gold process, it there a test method
abbreviated as "DMG" for testing gold porosity/Ni migration? Also besides
the three test methods as described in IPC-TM-650 2.24 for gold porosity, is
there any other test methods commonly used for ENIG in the industry?
Any advice is appreciated.
Best Rgds,
Darik Leung
Mica-AVA / QA