I have seen this with vme connectors. It was due to connector not allowing
the board to expand at the same rate as the material around it. We ended up
using a stiffener that held the board and the PCB and did not hard attach
the connector to the board ( i.e did not screw it down till after it was
soldered.
jg
-----Original Message-----
From: [log in to unmask] <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Friday, December 11, 1998 10:29 PM
Subject: [TN] Warped boards at PCI connector?
>To technet
>I have this board that is 18 by 14 though hole and SMT. After reflow the
board
>looks good not warped. Once assembled and sent to wave the board warps,
only
>around the PCI connectors. It warps so bad I don't have any lead
protrusion. I
>have tried to run this board many ways fast slow and minimal preheat. I
still
>have this problem. Has anyone ran into this problem before? Is this common
>around PCI connectors? I recall this happening once before many years ago,
I
>resolved it by tacking down the edge and middle of the connectors then
>masking. Is this the only fix? Any other suggestions
>
>Thanks in advance
>Angie
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|