Hello Techies,
I have a couple of questions on gold bath analysis. We
currently use the gold prospector from Dynatronix. Since they are no
longer making these nor supplying test solutions I was wondering what
the alternatives might be. I know of the gravimetric method utilizung
Nitric and Sulfuric acids but my Lab operators have some major
heartburn with this.
Thanks in advance for the help.
Mike Doty