Tom,

One additional question also to consider before presenting recommendations:

What is the lead length extension past the printed circuit board?

Mary Smoot
Process Engineer
Lexmark Electronics
Lexington, KY
[log in to unmask]



[log in to unmask] on 12/09/98 01:11:43 PM

Please respond to [log in to unmask]; Please respond to
      [log in to unmask]

To:   [log in to unmask]
cc:    (bcc: Mary Smoot/Lex/Lexmark)
Subject:  Re: [TN] Solder bridges during wave soldering




Hey Tom,

Let's see if I'm first with more questions.
I think more data is needed prior to answering your questions.
What is your pot temp?
What is travel speed?
What is the profile for temp rise?
What is pad stack and distance between pads on bridged joints?
Is this a new design or has something else changed in your process?
Feel free to call if you would like.
Talk to ya soon.
FNK

Frank N Kimmey C.I.D.
EM Designer
C&K Systems, Inc.
916-353-5366
[log in to unmask]

> ----------
> From:         Fawn Industries, Elm City
> Plant[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;Fawn Industries, Elm City Plant
> Sent:         Wednesday, December 09, 1998 9:48 AM
> To:   [log in to unmask]
> Subject:      [TN] Solder bridges during wave soldering
>
> Technetters,
>
> We have an Electrovert Wave soldering machine, that does not use a hot
> air
> knife, we wave solder alot of PCB's with good results.  We have one
> particular PCB that exhibits solder bridging on some through-hole
> transistors.  Can anyone offer some suggestions, it would most
> helpful!
>
> Thanks
>
> Tom Braswell
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2