Try Indium Corporation at 315 853 4900
Regards
Gerard O'Brien
Photocircuits
-----Original Message-----
From: James Kittel [SMTP:[log in to unmask]]
Sent: Monday, December 07, 1998 10:12 11:05
To: [log in to unmask]
Subject: [TN] Solder Balls for BGA's
Anyone know of a source for replacement eutectic solder balls for BGA's?
I need 0.0295 inch dia balls (0.75 mm).
Thanks,
Jim Kittel
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|