Michael, a couple items here might put this in perspective.
1) Fused T/L is much more costly to produce for the fabricator.
2) T/L does not fuse below 300 micro in.
3) The metal is not Eutectic. 60/40 only. (watch that plastic range)
hope this helps,
Mark Simmons
################################################################