Ryan,
I asked the same question to an Environmental / Civil Engineering Professor at the University Of South
Florida. The only attempted use that he was aware of was one in which the scrap PWB's were shredded and
mixed with asphalt for a road surface called "Glasphalt". The only problem was the material turned out to
be to abrasive to tires and thus was never used.
Craig Smith
Process Engineer
Paradyne Corporation
Ryan Jennens wrote:
> Mornin' everybody!
>
> Is there a good way to dispose of above subject? I don't think we can just
> pitch 'em 'cause they have lead on the pads. There has to be somebody that
> can grind 'em up or something. Maybe we could even make a little $? Thanks
> all.
>
> Ryan
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|