TECHNET Archives

December 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Teo Tijerina <[log in to unmask]>
Date:
Thu, 17 Dec 1998 15:58:49 -0700
Content-type:
text/plain; charset=us-ascii
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (25 lines)
Ladies & Gentlemen:
     I am trying to initiate test IPC-TM-650 in my wave solder machine to
test for the presence of halides in a "halide-free" no clean flux.  I have
had issues with cross contamination of water soluble and no clean flux due
to operator error (ie. the operator accidentally dumps water soluble flux
into a no clean flux bath).  IPC-TM-650 calls for the use of silver
chromate test paper.  Does anybody know where I can get some of this paper?
Anybody have any ideas on how to prevent cross contamination of fluxes

-Thanks,

Teo Tijerina

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2