Jim :
Here are a few treatments in order of bond strength:
1) There is a Boeing procedure that is based on a Phosphoric
anodizing process that is exceptionally good. Remember
to get the material unsealed as the sealing compound will
prevent good adhesion. ( should be listed under an
ASTM spec)
2) If you require less adhesion then a commercial Phosphate
treatment will work .
3)If you want to do the work in house then try a degrease bath
followed by a pumice slurry to roughen the surface with a
subsequent dry before bonding.
----------
From: Jim Marsico 516-595-5879
To: [log in to unmask]
Subject: [TN] SURFACE PREPARATION OF ALUMINUM
Date: Friday, December 04, 1998 11:21AM
I'm looking for a procedure to prepare a cast aluminum (A356) core for
epoxy
bonding to a polyimide PWB. Any Recommendations?
Jim Marsico
AIL Systems Inc.
(516) 595-5879
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
|
|
|