Yep. Especially if this is a Plastic BGA. I've had rework problems
where my ramp was too fast causing the substrate to warp slightly
which caused my shorts.The overmold is more thermally stable. That's
why it was occuring only on the corners. A more conservative profile
particularly during the soak stage fixed the problem.
-Dave
-----Original Message-----
From: MChan
Sent: Thursday, December 10, 1998 9:35 AM
To: TechNet
Cc: MChan
Subject: Re: [TN] BGA short
check the warping of the BGA PWB carrier pre and post reflow.... as the
PWB
warps, it may be pushing the solder...another check point may be your
stencil
design/process....
Marcelo
-----Original Message-----
From: Poh Kong Hui [SMTP:[log in to unmask]]
Sent: Thursday, December 10, 1998 10:07 AM
To: [log in to unmask]
Subject: [TN] BGA short
Hi Technetters,
I am facing a weird problem.
One of the board that we make, is having short underneath the
BGA.
However, every single short is always at one of the 4 corners of
the BGA.
Is there anyone facing such an issue ? Could someone advise me
how
to solve.
Poh
################################################################
TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask]
with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line
Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask]
or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
<< File: Re_ [TN] BGA short.TXT >>
|
|
|