Technetters,
This is reposting of my earlier call for help, with some additional info
asked by Frank K.
We have an Electrovert Wave soldering machine, that does not use a hot air
knife, we wave solder alot of PCB's with good results. We have one
particular PCB that exhibits solder bridging on some through-hole
transistors. Can anyone offer some suggestions, it would helpful!
>>Hey Tom,
>>Let's see if I'm first with more questions.
>>I think more data is needed prior to answering your questions.
>>What is your pot temp?
>>What is travel speed?
>>What is the profile for temp rise?
>>What is pad stack and distance between pads on bridged joints?
>>Is this a new design or has something else changed in your process?
1. What is you pot temp?
490 F
2. What is your travel speed?
4.0 in/min
3. What is profile for temp rise?
200-210 f until wave with Kester 951 no-clean.
4. What is pad stack and distance between pads on bridged joints?
Less than 1/2mm between pads on staggered layout, with 1mm lead
protrusion
5. Is this a new design or has something else changed in process?
Yes, this is new design PCB is 7in x 6 in, overhang of components
dictates that PCB can not be rotated 90 and waved.
Thanks! Thanks Frank!
Tom Braswell
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|