Dear Technetters,
Currently we have changed to use PCB with OSP (Organic
Solderability Preservative) finished instead of HASL (Hot Air
Solder Leveling) finished, the PCB is a single side one, CEM-1
or CEM-4 material, mixed technology with through hole and
surface mount component, which then go through wave soldering
process. The PCB itself has some big copper land/trace design
for high current flow which patterned with circular opening by
solder resist in order to increase overall trace thickness but
not create solder coalesce problem, the circular pads is 1mm
in diameter and with 1.5mm centre to centre distance. After
the wave soldering, all the through hole lead solder joint and
surface mount device seems no difference in quality when
compare with the HASL finished board, but a random solder
skipping happened on those circular pad opening, the skip
solder area can be readily take up solder by applying solder
wire with solder iron, the question is :
1. What is the root cause of such problem? Flux (the flux
using is a rma no clean type)? Machine setting? Pad design or
others?
2. The way to eliminate this problem, but if it cannot,can we
just let the skip solder pad (with copper expose) remain
unsolder, will this create reliability problem? What I heard
from some of the OSP supplier that this should be OK.
Thanks in advance,
WM Cheng
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|