This is theoretically possible... We have a design we are reviewing prior to
testing that will carry 40-50 amps continuos. We achieved this by creating
extremely wide traces and selectively plating them to 0.030 thick (much
thicker then even 3 ounce copper). You might try contacting Speedy Metro
(sp?) for information on the selective plating design.
Jeffrey A. McGlaughlin
PCB Designer
Battelle Memorial Institute
Columbus Ohio
[log in to unmask]
-----Original Message-----
From: Dallara, Louis T (Louis)** CTR ** [SMTP:[log in to unmask]]
Sent: Wednesday, 16 December, 1998 13:21
To: [log in to unmask]
Subject: [DC] 60 Amp traces
Question;
Do you think its possible to run 60 Amp traces on pcb board. What
size
plated thru hole
would I need for a pin to carry that kinda current.
Whats the largest current anybody has used????
Thanks
Lou
Louis T. Dallara
Product Design Information (PDI) Group- Dept. 52R143000
LUCENT TECHNOLOGIES - MICROELECTRONICS GROUP
Optoelectronics Business Unit
Office: 2I-146E, 9999 Hamilton Blvd., Breinigsville, PA 18031
Telephone: 610-391-2145 FAX: 610-391-2142
e-mail: [log in to unmask]
This transmission contains information belonging to Lucent
Technologies and
may be confidential and/or legally privileged. The information is
intended
for the individual or entity named above. IF YOU ARE NOT THE
INTENDED
RECIPIENT, YOU ARE HEREBY NOTIFIED THAT DISCLOSING, DISTRIBUTION OR
COPYING
THIS INFORMATION IS STRICTLY PROHIBITED. IF YOU HAVE RECEIVED THIS
EMAIL IN
ERROR, PLEASE CONTACT THE SENDER NAMED ABOVE.
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|