John, paragraphs 8.4 through 8.8 of IPC-2221 gives a small amount of
guidance. Also check out the sectional spec's like IPC-2222, Rigid boards or
IPC-2223, flex boards.

Good luck

Thanks,
John H. Morton
Dept 574,  607-751-4990
[log in to unmask]
Lockheed Martin Federal Systems
MD 0306 1801 State Route 17C
Owego, NY 13827

> -----Original Message-----
> From: John Mastorides [SMTP:[log in to unmask]]
> Sent: 12 November, 1998 1:25 PM
> To:   [log in to unmask]
> Subject:      [TN] DFM for SMT Spec.
>
> Looking for a Document/Guideline containing Design for Manufacturability
> of
> SMT assemblies.
>
> Any suggestions?
>
> Thanks in advance.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2