Good Afternoon!
Can any of you tekkies out there help me, I wish to remove
the enamel coating from 0.008mm Cu/Mn/Ni wire. The present
method uses a Potassium Hydroxide solution mixed with
water, but does not remove the enamel sufficiently.
Thanks in advance
Pat Diamond
################################################################