Hi Jerry,
I don't know if this will help or not, but MIL-STD-2000A referred to a
fused electroplated Sn-Pb finish conforming to MIL-P-81728. I can't
remember the particulars with that spec but I do remember there was quite
a struggle in writing that solderability requirement to include other
lead finishes as an alternate to solder coating.
It only makes sense to me that the lead finish should be compatible with
the eutectic Sn-Pb solder and process temperatures (assuming reflow or
wave) while still providing the ability to maintain solderability. But
then, component mfr's are more concerned with efforts to reduce/eliminate
lead and qualify for environmental awards and other government kickbacks
(I know what you think of TI's Pd-Ag) than working with the masses.
Steve Sauer
Sr. Mfg. Engineer
Xetron Corporation
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|