TECHNET Archives

November 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Tue, 10 Nov 1998 09:52:25 -0600
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (34 lines)
     Can anyone assist me on the following.  Thanks.
     
     Address,
     
     This is for the asssembly houses.  When using Immersion Tin, is it 
     necessary to bring the oven temperature to the melting point of Tin 
     (232°C).  Will the Sn dissolve into the Eutectic solder deposit via 
     solderpaste deposition, if so, at what temp.  Can anyone provide 
     experiences.
     
     I am using Kester' WS851 (R596) for solderpaste.  This is a Halide 
     free paste.  Does anyone know if this is incompatible to using 
     Enthones Entek 106A OSP?  Should I be using a Halide baring paste 
     (ORM1) to remove the OSP finish?
     
     Detailed information required!!!
     
     
     Thanks.
     
     John Gulley

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2