Howdy all-
Three more days!
When I asked our board fab house to mask the vias on the bottom side of one
of our boards to avoid the shorting which has been plaguing us, I was told
that they could do it, but for a cost of thousands of $. They said that
they would have to make a clamshell fixture to test the bare board before
they ship it to us. What are my other options for avoiding shorts to these
vias which are near pads. This happens under BGA parts and also near some
surface mount parts. Is tenting more than just covering the vias with
solder mask? Thanks in advance for the wonderful insight which always
follows these inquiries!
Ryan Jennens
Phoenix Engineering Design, Inc.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|