Ajay,
Sheen is a UK manufacturer of a whole range of test instruments.
In case you dont have access to it, their address is
Sheen Instruments Ltd
Unit 4 St George's Ind Est
Richmond Road
Kingston KT2 5BQ
Tel: +44 181 541 4333
Fax: +44 181 549 3374
In answer to your question, the cup you refer to is Ref 401 Conforming to
BS3900:A6,1971 Number B4.
You should however, be able to use either a Zahn #3 or a Ford #4 cup, which
might be easier for you to obtain.
The cup test involves filling the cup with the coating material, setting
your stopwatch as it is taken out of the coating (the cup that is, not the
stopwatch!) and timing it to drain out. This should take, as you state, 24
seconds +/- 2 seconds. Exciting isn't it? Ah, the miracle of science at
work!
Some other TechNetter may be able to point us all to a web address that
provides a flow cup comparison table?? Anyone care to help?
Regards, Graham Naisbitt
[log in to unmask]
Concoat Ltd Phone: +44 1276 691100
Alasan House Fax: +44 1276 691227
Albany Park
CAMBERLEY
GU15 2PL UK
Any opinions expressed are those of this employer.
-----Original Message-----
From: ajay agarwal <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: 19 November 1998 01:03
Subject: [TN] conformal coating[SHEEN CUP 401/4 specification]
>Techneters,
>One of our customers want us to use two component conformal coating and
>asper that we need to thin the coating using some thiner to meet a SHEEN
>CUP 401/4 specification with draining of 24 seconds +/- 2 seconds.
>I want to know about this SHEEN CUP specification and actual procedure
>to perform that.
>Any help will be highly appreciated.
>Thanks
>Ajay Agarwal
>
>
>______________________________________________________
>Get Your Private, Free Email at http://www.hotmail.com
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|