Moti,
there was no intention to discredit anyone - intent was to display that - with
all due respect to the other alternatives - ( additives will only take u so
far in DC mode ) - there is a better alternative - and it is viable - as
someone once wrote about DC plating -
quote : " virtually all the plating equipment designed to accomodate the
simpler panels of the 70's n 80's is now unable to produce the same throughput
when running today's more complex boards." unquote