Francis,
How long of a dwell time and at what temperature is the gold plating
solution operating at? The solutionitself is fairly aggressive on dry
film.Some companies manufacture a film just for this application.
Good luck,
-----Original Message-----
From: Francis Lai <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Friday, November 06, 1998 4:40 PM
Subject: [TN] Problem in Gold Plating
>I work in gold plating. We are using electrolytic gold plating.
>
>It is pattern plating. However the gold leaks underneath the dry film.
>
>As a result the pattern is fatter after the dry film is removed.
>
>We develop the pattern dry film and thenn hardenn the dry film by
>
>exposing under UV light again. But still it leaks underneath the dry
>
>film. Could any one help ?
>
>WE also want to set up a pulse plating bath ourselves. Could any
>
>one give us some information onn how to start ?
>
>Thanks in advance!!!!!!!!
>
>my e-mail : [log in to unmask] ( Please do not send graphics, this
> is text base)
>
>Thanks again
>
>Francis
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|