Interesting idea, isin't it.
I have just begun this evaluation having installed a dozen or so of these
fingers on an Electrovert Econopac about three weeks ago. So far the
results are very positive with no breakage, deformation or distortion. The
finger cleaner also seems more effective but this benefit may evaporate as
the fingers age. I will convert one wave solder machine over to polymer
fingers as soon as I can get them in.
Regards and good luck,
Brad Vanderhoof
-----Original Message-----
From: Jerry Cupples [mailto:[log in to unmask]]
Sent: Tuesday, November 24, 1998 8:15 AM
To: [log in to unmask]
Subject: [TN] assy: wave solder fingers
I would be interested in corresponding with anyone who has tried
glass-reinforced polymer conveyor fingers (replacement for Ti) in a
wavesolder application.
A local company called JAFCO is offering these. Actual experience is what I
want to know about; I have an infinite supply of speculative opinions here.
regards and happy turkey fest,
Jerry Cupples
Interphase Corporation
Dallas, TX USA
http://www.iphase.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|