Ingemar:
To determine if Marianne's suggestions are correct, in my experience,
the best way would be to perform thermodynamics analysis on the
materials. A thermomechanical analysis (TMA) will tell you Tg, as well
as give a feel if the material is properly cured if the correct
techniques are employed during the analysis. Residual stresses can also
be found using DMA; TGA analysis might be helpful if you have a
hydroscopicity problem causing registration losses...
Regards,
> Bill Davis, Ph.D.
> Diamond Multimedia Systems
> Senior Scientist
> Tel. 408.325.7868
> Cell. 408.888.5650
> e-mail: [log in to unmask]
>
>
>
>
> -----Original Message-----
> From: [log in to unmask]
> [SMTP:[log in to unmask]]
> Sent: Thursday, November 19, 1998 11:43 PM
> To: [log in to unmask]
> Subject: Re: [TN] THERMOPLASTIC RELIABILITY
>
> >Thanks for answer, Marianne,
> I will ask the manufacturer as you indicate. Werner Engelmaier is of
> different opinion. He thinks we exaggerate the problem. Huge and heavy
> and complex structures are being built with thermoplastics, and they
> keep adhesion despite hot ambient conditions. Thanks again.//Ingemar
>
> --------------------------------------------------------------------
> No optimism here.
> >
> > If the maximum Tg is 75 C, it is quite possible that the beginning
> of
> the
> > glass transition zone is in the 60 C range. Softening and loss of
> > positional registration can therefore occur.
> >
> > To verify whether this particular product is useable in your
> operating
> > environment, you may want to have the material analyzed to determine
> where
> > the onset of softening occurs, and to ask the supplier for their
> > manufacturing process tolerances on the thermoplastic. Or run your
> product
> > through reliability testing.
> > ____________________________________________________________
> > Marianne Romansky
> > Process Development Scientist
> > Celestica (Toronto) Inc.
> > Phone: (416) 448-6284
> > Email: [log in to unmask]
> >
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|