TECHNET Archives

November 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Fri, 20 Nov 1998 04:04:02 -0600
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Colin <[log in to unmask]>
Parts/Attachments:
text/plain (47 lines)
Technetters,

I have an issue with the Mil spec MIL PRF 55110 F, which states that if you
see lifted lands in the microsection, that you then inspect the lot 100%
visually for seperation at 4X mag. and if not seen then the boards should
be acceptable.

I have to requalify using the 10 layer multilayer pattern of the MIL spec.,
but have not been able to do so due to minute cracking of the resin under
the pad, at the resin/glass interface, seen only at microsection at 200X.
It is not visible to the naked eye, or at 4 X. (I have a photo if required,
but have not attached it here due to bandwidth. besides, I don't want
spammed!- mail me if you need a copy please)but the requalification people
are insistent that as it is pad lift, although only seen under
microsection, it must fail. So when is pad lift not pad lift according to
the specification, or vice versa ?????

The PCB's are "as received", having only been HASL'd. Several "fixes" have
been tried, including reduction of copper plate thickness in the holes,
change of bonding prepregs from 1080 to 2113/2116 to reduce the resin
content, electroless copper instead of direct plate, higher Tg materials
instead of standard FR4, change of HASL temperature and dwell, ductility of
copper etc. (not all at once of course)

I am at a loss to explain this, especially on the requalification issue,
and am sure that several other fabricators have experienced this issue before.
What was the outcome, and what was the answer?

Hope someone can shed some light.

Colin William

"Opinions expressed above, are just that, and are my own, and do not
reflect those of my employer"

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2