TECHNET Archives

November 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7Bit
Sender:
Subject:
From:
Chen Fung Leng <[log in to unmask]>
Date:
Tue, 17 Nov 1998 17:49:24 -0800
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
Chen Fung Leng <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Hi,

I would like to find out if there are any non wetting agent for epoxy based
encapsulation material.

Basically, I would like to coat such a material onto a surface to prevent
epoxy-based material from wetting it. It would be great if such a coating
material could be removed subsequently.

I would appreciate if anyone could advise.

Best regards,
Fung Leng

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2