No optimism here.
If the maximum Tg is 75 C, it is quite possible that the beginning of the
glass transition zone is in the 60 C range. Softening and loss of
positional registration can therefore occur.
To verify whether this particular product is useable in your operating
environment, you may want to have the material analyzed to determine where
the onset of softening occurs, and to ask the supplier for their
manufacturing process tolerances on the thermoplastic. Or run your product
through reliability testing.
____________________________________________________________
Marianne Romansky
Process Development Scientist
Celestica (Toronto) Inc.
Phone: (416) 448-6284
Email: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################