It certainly must be lonely at the top, as in outer space, with the stuff you are doing. I use
ANSI/J-STD-001 and its table 5-1 as a guide to determine whether a specific contamination
level is exceeded in the solder. For applications using immersion gold, in a thickness not
exceeding 7 millionths", the rule is not violated for most SMT solder paste and joints.
Does 5 microns exceed the limit when corelated with your solder amount and the aforementioned
rule? If so, do as must be done and remove the gold in a solder pot (not contaminated with too
much gold - of course). Then, perform the soldering operation safely while expecting initial
solder joint acceptability, and long term reliability without embrittlement and subsequent
failure.
Earl Moon
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|