Hello, Jos.
Ceramics is not my specialty, just happened to get into it a little when
we had (and still have) some strange problems with ceramic components.
Pb seem to be used in a group of ceramics called Relaxor Dielectrics.
Typically these material can be sintered in as low temperatures as 950
degrees Celcius. Example:
Pb(Fe2/3 W1/3)O3 - PbZrO3 plus MnO2 with k´>5,000, tan
delta 0.01 and Ris approx 10exp10 Ohm-cm.
O.Iizawa, S.Fujiwara, H.Ueoka 1980.
There are certainly hundreds of technicians you can call for mor
information. For instance AVX/Kyocera, Coors and many more.
As I said, just happened to get a few lines under my eyes about the
issue. Good luck!
//Ingemar Hernefjord
Ericsson Microwave Systems
> Hello,
> We are using electronic components containing Pb as metal but
also Pb
> as oxide or Pb-titanate in ceramic components. It is clear to me
that
> Pb as free metal will be phased out, but is there some (draft)
> legislation for Pb-compounds in ceramics?
> Jos
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text
> in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for
> additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700
> ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|