Hi Bryan,
Contact East sells a touchup pen called "Circuit Works". It is just the
thing you need for your application.
Good Luck
Bruce Adams
Datametrics Corp.
Orlando, FL [log in to unmask]
> -----Original Message-----
> From: Bryan Bloom [SMTP:[log in to unmask]]
> Sent: Tuesday, November 10, 1998 11:54 AM
> To: [log in to unmask]
> Subject: [TN] fixing exposed copper/traces
>
> With a through-hole board, somtimes the masking is nicked, exposing
> the
> copper (bare metal).
>
> What methods - pens, etc. - do others use to touch up the mask? Any
> recommendations on specific products (manufacturers) and/or methods?
>
> Thanks for your help.
>
> Bryan Bloom
> G&M Assembly
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|