It is not a good idea to use pure tin on electronic devices because of
whiskers/dendrites. See IPC-TR-476 first...
Paul Signorelli
RW Systems
[log in to unmask]
_______________________________________________________________________________
_
From: TechNet on Wed, Oct 21, 1998 07?39
Subject: Re: [TN] pure tin surface finish require
To: [log in to unmask]@inetgw
In a message dated 98-10-21 01:17:39 EDT, you write:
<< Hi All,
I got some inquirty from customer. They want us to use pure tin as
surface finish treatment. Is there any resource that can help me to get
this order? I am very appreciated if you can provide any information to
me.
>>
How much pure Tin do you need?
There is immersion Tin, which, depending on who's lies you believe, can give
you 30-100 microinches, or electrolytic plating, which can give you as much
as
you want, but is a serious hassle to figure out how to do.
Rudy Sedlak
RD Chemical Company
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|