Has anyone experienced LED failures while running product through a wave
solder? I am having some fallout on some LED's. The component spec.
states that it can handle solder temperature of 260
°C for 5 seconds. My
solder pot is only at 250°C and a dwell time of 2 seconds. Can anyone shed
some light on this subject for me?
Rob
[log in to unmask]