Ryan Jennens wrote:
> Mornin' all!
>
> We have a problem with our through-hole lead cutters dulling. They are
> the hand-operated type as we are hand-stuffing through hole parts for
> now. They are just your run-of-the-mill clippers, and I cannot find any
> specially hardened versions to last longer. Our leads are not made of
> any particularly hard material. Is there a different solution than
> buying new clippers as they wear out? Thanks again.
>
> Ryan
> Phoenix Engineering Design
Ryan,
You might try Kline <--sp for you tool supplier. I have had
very good results with their tools for electronics work. I don't do
assembly any more but Kline had a cutter that is hardened on the tips
only. The cutters were about $12.00 or so, (4 or 5 years ago) but they
worked great. The only time I had one fail was when a Engineer cut Stainless
steel wire that was about a 18 ga. and the tip turned into a stripper then
broke. I was gone the day he used them for that or I would be writing you
this from prison....... The moral of the story of course is, NEVER let an
engineer use any tools except a pen or pencil! (I'm going to get hammered
for that statement...) Anyway, try Kline for your cutters and their was
a Swiss company that made some also but I don't remember the name. Very
expensive though, $30.00 + bucks but also very good. If you need the name
send me mail off-line and I'll check at home for the name.
Later.
--
Scott Decker
AKA: PadMasterson
Praegitzer Design On Location at
Enterprise Server Group CO3
Intel Corporation
Ph: (503)-677-6582 E-MAIL: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|