I have been informed that several fine coats rather than one
thicker coat improves adhesion, however, I have no practical
experience of it to back this up. Might be worth a try, but it
will increase your process time. And yes, cleanliness is an
issue. i suggest you approach your supplier.........Bridget
> -----Original Message-----
> From: Paul Stolar [SMTP:[log in to unmask]]
> Sent: 12 October 1998 15:09
> To: [log in to unmask]
> Subject: [TN] Confomal coating adhesion
>
> *** WARNING ***
>
> This mail has originated outside your organization,
> either from an external partner or the Global Internet.
> Keep this in mind if you answer this message.
>
>
> Does anyone have any good experience at improving
> conformal coating
> adhesion to plastic packaging?
>
> Is it a cleanliness issue, or is it inherent in materials?
>
> ###############################################################
> #
> TechNet E-Mail Forum provided as a free service by IPC using
> LISTSERV 1.8c
> ###############################################################
> #
> To subscribe/unsubscribe, send a message to [log in to unmask]
> with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ###############################################################
> #
> Please visit IPC's web site (http://www.ipc.org) "On-Line
> Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask]
> or 847-509-9700 ext.312
> ###############################################################
> #
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|