Chris,
Alpha PC Fab still carries Sealbrite product line.  Please call Anita
Gillanders at (949) 757-0111, x4516 for details.

Best regards.

Eric Yakobson




mark ross <[log in to unmask]> on 10/08/98 11:08:17 AM

To:   [log in to unmask]
cc:    (bcc: Eric Yakobson/AlphaPCFabUS/Cookson)
Subject:  Re: [TN] Sealbrite




We use Dynacircuits outside of Chicago and I went to their web page on an
unrelated item and happened
across sealbrite listed as a coating still available under their
capabilities section.  You can go to
www.dynacircuits.com for further info on how to contact them.  I don't know
for sure they still have this
as an option but since it was used in cost sensitive markets and they make
single and double sided boards,
they may be able to steer you towards something.


Mike Barmuta wrote:

>         Chris: Since LONCO was bought out (about 10 years ago?)I don't
believe
> Sealbrite exists anymore. Alpha Metals did carry some similar products
that were
> non activated modified rosins. There was a 300 series that had various %
solids
> depending on your aplication method also two other products 828 and 2301
that a
> different solvent carrier system to allow lower temp drying. The west
coast phn#
> for Alpha is 949-757-0111.
>         If these are not available you could "probably" use a straight R
rosin
> flow soldering flux.
> This is "messy" stuff to work with, if the application is for Cu PCB's I
would
> suggest you try to get your customer to go with one of the newer
generation
> OSP's.
>                                                 Regards
>                                                         Michael Barmuta
>                                                         Staff Engineer
>                                                         Fluke Corp.
>                                                         Everett Wa.
>                                                         425-356-6076
>
> On Wed, 7 Oct 1998 11:08:51 -0700 Chris Williams wrote:
>
> > From: Chris Williams <[log in to unmask]>
> > Date: Wed, 7 Oct 1998 11:08:51 -0700
> > Subject: [TN] Sealbrite
> > To: [log in to unmask]
> >
> > Remember Sealbrite?  It's no longer made, but we have a customer that
is
> > very interested in using it.  Does anyone know of a good alternative or
> > replacement?  Thanks in advance.
> >
> > Chris Williams
> > Graphic Products, Inc.
> > [log in to unmask]
> >
> > ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> > ################################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
following
> text in the body:
> > To subscribe:   SUBSCRIBE TechNet <your full name>
> > To unsubscribe:   SIGNOFF TechNet
> > ################################################################
> > Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section
> for additional information.
> > For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> > ################################################################
> >
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2