Rick,
I cut my teeth on this type of SMT assembly, many (we won't say how
many) moons ago. Ceramic is more fragile and a better heat sink then
typical FR4, so you may have to allow more time to ramp, time at peak,
and slower cool-down, to avoid cracking, especially if substrate
thickness is less then .030", and/or board is larger then one square
inch. The type of conductor used for the traces may be a concern also
(pt/pd/au? pd/ag? thickfilm vs. other?). Other then a few concerns
like this, it actually can be a very robust process. Please give more
info, or call me directly, and I'll be glad to answer any process
questions.
United Technology Electronic Controls
Jeff L. Hempton, Sr. SMD Engineer
Phone: 219-359-3514
E-mail: [log in to unmask]
______________________________ Forward Header __________________________________
Subject: [TN] SMT Assembly on Ceramic substrate?
Author: Rick Thompson <[log in to unmask]> at Internet
Date: 10/27/98 9:07 AM
Hi,
One of our customers has asked us to look at assembling smt components on
ceramic substrate for them. This is a process that we have no experience
with. If anyone can offer information regarding this process, things to
watch for, etc. it would be greatly appreciated.
TIA
Rick Thompson
Ventura Electronics Assembly
2665A Park Center Dr.
Simi Valley, CA 93065
[log in to unmask]
(805) 584-9858 voice
(805) 584-1529 fax
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|