Good morning Weemei -
In response to your questions:
1] Yes, it is true that solder will flow thru a via, when that via is placed
in a component termination pad. This results in a condition where solder is
stolen from the intended termination, resulting in an insufficient solder
connection. In turn, a portion of that solder fills the via, and a bead may
form on the opposite side of the circuit board. This was a design technique
that many of us tried in the late 1980's and discarded as a result of the
problems noted above.
2] The vias we experienced this problem with were in the .012-.018" finished
inner diameter range. I have not experimented to determine whether a small
enough via could be created to prevent capillarity. Given the flow
charactaristics of molten solder, I suspect this could not be accomplished in
a manner that can be repeated consistantly under production conditions.
Since proven design alternatives exist, this would seem to be an entertaining
science project with little or no practical application.
3] As noted in item 2 above - I have no answer for this question.
Regards - Kelly
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|