Hi
We are running in our plant Electroless nickel - Immersion Gold ( ENIG )
finishing for PCB based on Atotech chemistry . Phosphour content is in
middle range ( average 9% ) .
One of our customers request low phosphour content - less than 7% .
We ae trying to force the chemistry to plate Nickel with such content of
phosphour by rising the temperature , increasing volume load ( sq cm per
liter of working solution ) etc , but untill do not have stable process
parameters .
Any recommendation for Atotech chemistry or someone else chemistry ???
Edward Szpruch
Eltek Ltd - Israel
Tel 972 3 9395050
Fax 972 3 9309581
E-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################