We use Hot Bar soldering to attach Flat Ribbon Cables to PCB's.
We use Palomar Products (www.palpro.com) (formely Hughes) equipment,
also TODDCO has equipment. I read that Palomar now owns TODDCO.
Another equipment manufacturer is AIT (www.a-i-t.com).
The main issue with this process is the fixturing and if you use
solder quick tape (tape with solder) is easier but expensive. The
equipment suppliers can give you more information of this.
Mauricio Castro
______________________________ Reply Separator _________________________________
Subject: [TN] Hot Bar Soldering
Author: [log in to unmask] at INTERNET
Date: 10/6/98 9:24 AM
A recent SMT magazine contained an article on hot bar soldering. I am
searching for information on this process.
1) Equipment and manufacturers
2) Process
3) Design Guidelines
If anyone is currently using this process or has experience with it
and could provide me with some information I would appreciate it.
-David Bruni
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|