Hi Patty,
We use a Hughes welder as Ed recommended and it does work well but the Kovar
ribbon is expensive and it needs a good operator. There is another
alternative made here in the UK which uses copper ribbon. It is much easier
to use because it automatically delivers the exact amount of energy to make
the weld so you don't have to adjust anything. We had to rent one when our
Hughes needed repair and it worked well plus the copper ribbon is much
cheaper. The manufacturer is Seetrax Ltd and their telephone number is ++44
1730 260062.
By the way we ran out of the 6 mil and 10 mil Kovar ribbon. If anyone knows
of a source I'd be grateful. Delivery is 4 weeks at the moment. Luckily we
don't need to use it much otherwise I would buy the Seetrax machine.
Paul Gould
Teknacron Circuits Ltd
-----Original Message-----
From: Causey, Patty - LYPME <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: 29 October 1998 13:05
Subject: [TN] fab: repair inner layer trace
>After an inner layer has come out of the etcher and you find a trace
>that is broken, is there anyway that you can repair a copper trace (easy
>access to it, i.e., not close to any other traces) that will withstand
>the subsequent lamination cycle?
>
>Thanks,
>
>Patty G. Causey / LYPME
>Manufacturing Engineering Support
>(912) 926-9473 DSN: 468-9473 Fax: (912) 926-7974
>email: [log in to unmask]
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|