Hello everybody
I would appreciate if somebody could please help me with the following:
1.0 where could i find information about the wafre dicing practices used
in the industry.
2.0 After the dicing opration is completed, the dice are placed in the
waffle packs. What kind of pick up tips are used to transfer the dice
from the wafer to the waffle packs.
3.0 Would the transferring of the dice from the wafer to the waffle pack
introduce damage to the top side or the back side of the dice.
4.0 What are the current practices used in the industry in order to check
those damages. In other words hw does one assure a defect free prodcut to
the customer.
Knowing the above is kind of urgent for me. Therefore,
Any help in this regard would be greatly appreciated.
Regards
Manish
----------------------------------------------------------------------------
Those who do not remember the past regret it, Those who misremember
the past repeat it as a proof.
----------------------------------------------------------------------------
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|