Good morning Gary,
Seal Labs in El Segundo CA has always done a good job with work I have sent them.
If it is a small job stop by and we may be able to take care of it in house for you.
See ya,
Brad

-----Original Message-----
From:   [log in to unmask] [SMTP:[log in to unmask]]
Sent:   Tuesday, September 01, 1998 5:35 PM
To:     [log in to unmask]
Subject:        [TN] FAILURE ANALYSIS LABORATORIES

Good Evening, TechNet Recipients!

I am trying to locate reputable IC failure analysis laboratories with
facilities to remove lids and perform a detailed failure analysis of failed
SMT power devices.
Prefer West Coast locations.  Any suggestions?

Thanks for your assistance.....

Gary Moravchik
Production Technology
"[log in to unmask]"

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2