Paul,
Better check those Jedec Specs again! I'm very certain the numbers in the
specification are in one direction. In other words 0 to 4 mils not +/-4
mils. Makes a big difference!
Now the manufacturer has the problem, not you.
Just for the record our company does coplanarity repair if you need us.
Regards, Russ
-----Original Message-----
From: Paul Stolar <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Monday, September 21, 1998 1:57 PM
Subject: [TN] Planarity
> Is anyone else having problems with the Jedec planarity standard of
> +/- 4 mils for fine pitch parts?
>
> The problem we have is that the spec of +/- 4 mils means that one can
> have an 8 mil planarity problem. If we have the paste thick enough to
> compensate, we get shorts.
>
> Is anyone working on tightening the spec?
>
> If any component guys are out there, what are your thoughts?
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|