Hi Mike,
Uncured solder mask will surely do it, I suspect that is your problem.
Regards,
Les
> From: Mike Manwell <[log in to unmask]>, on 9/17/98 9:26 AM:
> Hi and thanks for reading this message.
>
> Has anyone experienced solder "webbing" or "sticking" to the permanent
> solder
> mask on boards after wavesolder? I'm seeing it on some products but not on
> others. I suspect that it is uncured solder mask but wanted to get some
> other
> opinions.
> Thanks in advance,
> Mike
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|