Robert-
Sounds like the core is not symmetrical w.r.t the core centerline. Bet
you have a lot more Cu on the ground side of core than the signal side
(?) Does eyeballing the artwork for these 2 layers confirm this?
-Michael Alderete
You wrote...
------------------------------
Date: Wed, 16 Sep 1998 17:02:37 -0700
From: Robert Jordan <[log in to unmask]>
Subject: Warpage @ Assembly
Greetings,
I would like to ask for some insight with respect to an assembly
process.
I am trying to get a handle on why a 4 layer board would warp @
assembly.
The panel is really an palletized array of two boards, seperated by a 60
mil gap and attached @ five perforated ponits that join the panels
together. The board is manufactured using Allied's FR406. Construction
is
as follows;
6" x 9" board 9" x 12.1" array
.5 oz foil
Prepreg 2@7628 & 1@1080
Core .021 1/1 one side is a ground while the other side is circuit
related
@ approx. 5% coverage
Prepreg 2@7628 & 1@1080
.5 oz foil
The panels are pattern plated with 1-1.2 mil of copper in the holes
LPI SM Taiyo PSR 4000
Entek 106
The panels show no sign of warpage at our package stage/shipping
The panels are seeing two conveyorized reflows in a HotAir Unit? I am
not
sure if I have properly identified the assembly device. It does use hot
air
and not a solder wave.
The first pass thru the reflow involves some resistors, capacitors.
There
are no high profile components. This is layer 4. There is no sign of
warpage after this step.
The second pass with major components added resulted in 30% of the
arrays
warpping
------------------------------
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|