The test method for oxygen index, also called limiting oxygen index is ASTM D 2863. If you have access to
ASTM standards it is in volume 8.02, otherwise you can get ordering information at www.astm.org.
th_yeo wrote:
> Would appreciate help on the above.
>
> Understand that the definition of oxygen index (OI) is
>
> OI=(A/(A+B))*100
>
> A=oxygen flow rate
> B=nitrogen flow rate
>
> which specs does this come under and where could I get hold of the test method.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
--
John Moylan
President
Delsen Testing Laboratories, Inc.
1024 Grand Central Ave.
Glendale, CA 91201
Phone: 818 247 4106
FAX 818 247 4537
email: [log in to unmask]
URL: http://www.primenet.com/~delsen/
Delsen Testing Laboratories, Inc. is an independent testing
laboratory primarily engaged testing advanced materials.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|