TECHNET Archives

September 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Wed, 30 Sep 1998 13:02:03 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Hwang Steve-WLSH14 <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
Hwang Steve-WLSH14 <[log in to unmask]>
Comments:
( Received on motgate.mot.com from client mothost.mot.com, sender [log in to unmask] )
Parts/Attachments:
text/plain (49 lines)
Try reducing the RPM of the convection fans and lowering the temperature
of the bottom zones in your oven.


-----Original Message-----
From: Poh Kong Hui [mailto:[log in to unmask]]
Sent: Tuesday, September 29, 1998 5:30 PM
To: [log in to unmask]
Subject: [TN] Drop off Component


Hi Technetters,

I am facing with an issue that the component at the bottom side of
the board drop-off during the second-pass reflow process. However,
such incident happen randonly.

Could anyone advise me how to resolve such problem ? Thanks


Poh

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2