Adrian,
Check out Tom Peel at Contech Research in Attleboro, MA. The phone
number is 508-226-4800. We used to do quite a bit of work with them when
qualifying connectors systems (even PGA sockets) years ago. Check out
their website at:
http://members.aol.com/conres226
I also have a question for everyone: Do ISHM and IEPS still exist? Do
they have web sites? I did some searches recently with no luck. It's
been a while since I've looked into them.
Regards,
Paul Terranova
Here's my MS Outlook98 virtual business card:
Analytical and Environmental Test Services Lab
Phone: (508)467-3109
Fax: (508)467-6796
Email: [log in to unmask]
WebSite: http://www.digital.com/lab-services
-----Original Message-----
From: J. Adrian Riley [mailto:[log in to unmask]]
Sent: Wednesday, September 23, 1998 9:43 AM
To: [log in to unmask]
Subject: [TN] Test Lab for Corrosive Gas Testing
I am looking for test labs that can perform the "Flowing
Mixed Gas" or "Battelle
II thru IV" tests used for connector systems. Names &
phone #s, email or Web
addresses would be appreciated.
Thanks,
Adrian Riley
################################################################
TechNet E-Mail Forum provided as a free service by IPC
using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org)
"On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at
[log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|